Making pretty joints Lloyd E. Sponenburgh 05-02-2007
If you were  Registered and logged in, you could reply and use other advanced thread options
Posted by Lloyd E. Sponenburgh on May 2, 2007, 8:27 am
I have pretty good luck with brazing using Sil-Flo. The joints are strong,
don't leak, don't have much if any "drip".

But usually I have to clean them afterwards because Sil-Flo doesn't start to
flux and sweat well until almost to the boiling point, and that gets the
whole joint hot enough that there's lots of oxidation around afterwards.
Ken's joints look neater than mine, but still need cleaning.

I've always admired the joints I see in a new unit. I assume they're either
heated super-fast with a ring burner, or they are induction heated. You can
hardly see any discoloration, much less oxidization.

What rods do you guys use to make pretty brazed joints? Is Sil-Flo a bad
choice, or is my technique the problem?
What about tuning the flame? Reducing, oxidizing, neutral?

LLoyd



Posted by Bill on May 2, 2007, 3:39 pm
> I've always admired the joints I see in a new unit. I assume they're either
> heated super-fast with a ring burner, or they are induction heated. You can
> hardly see any discoloration, much less oxidization.

Factory joints use a torch that has flux in the flame.

Posted by Bill on May 2, 2007, 4:33 pm

> > I've always admired the joints I see in a new unit. I assume they're
> > either
> > heated super-fast with a ring burner, or they are induction heated. You
> > can
> > hardly see any discoloration, much less oxidization.
>
> Factory joints use a torch that has flux in the flame.

Picture of a factory rig. I forget the name of the maker.

http://surbsoft.com/HP.html

Posted by on May 2, 2007, 4:39 pm
wrote:

>> I've always admired the joints I see in a new unit. I assume they're either
>> heated super-fast with a ring burner, or they are induction heated. You can
>> hardly see any discoloration, much less oxidization.
>
>Factory joints use a torch that has flux in the flame.

        I thought they used Esmereldas ?


--
Click here every day to feed an animal that needs you today !!!
http://www.theanimalrescuesite.com/

Paul ( pjm @ pobox . com ) - remove spaces to email me
'Some days, it's just not worth chewing through the restraints.'
'With sufficient thrust, pigs fly just fine.'
HVAC/R program for Palm PDA's
Free demo now available online http://pmilligan.net/palm/

Posted by Bill on May 2, 2007, 8:31 pm
.p.jm@see_my_sig_for_address.com wrote:

> >Factory joints use a torch that has flux in the flame.
>
>         I thought they used Esmereldas ?

?
You talking about the torch tip? The clean joint is from the flux in the
gas.

Page 1 of 2       1 2 > last >>
Similar ThreadsPosted
OT. Romney sounds pretty good on Health Care August 3, 2007, 9:01 am
Another toy recall in the making ? October 15, 2007, 7:21 pm
making my air conditioner switch on a fan June 2, 2008, 7:11 pm
Heat pump making a clicking noise February 13, 2008, 10:21 pm
Crews making progress restoring natural gas to Buffalo, MN October 13, 2006, 6:28 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap